Carbon da aka kunna a cikin kwakwa na AuCarb™ Gold Recovery Shell (≥99% Taurin): Kinetics na sha, Kula da Hankali da kuma Ma'aunin Carbon na CIP/CIL

Tarar carbon ba ta da amfani sosai - ana ɗora su da zinariya daga da'irar. Karatun fasaha kan ƙimar K/R, riƙe raga da kuma ma'aunin carbon mai matakai bakwai.

Kusa da kusurwar harsashin kwakwa mai aiki da aka yi amfani da shi ta hanyar raga shida zuwa goma sha biyu da aka yi amfani da su don shaye-shayen zinariya a cikin da'irori na CIP da CIL

Littafin Fasaha · AuCarb™

Kinetics na shaye-shaye, Kula da Hanji da kuma Ma'aunin Carbon na CIP/CIL

Me yasa taurin ≥99%, yanke raga mai girman 6×12 da kuma raguwar ≤1.5% ke ƙayyade adadin zinare da aka ɗora a cikin da'irar - da kuma nawa ne ya rage a matsayin tarar.

Amsa da sauri

Carbon da aka kunna a cikin AuCarb™ Gold Recovery Coconut Shell Carbon (≥99% Tauri) wani nau'in carbon ne da aka ƙera don shaƙar zinariya a cikin da'irori na CIP, CIL, CIC, Heap leaching da kuma leaching na Vat. Aikinsa shine ya cire hadadden Au(CN)₂⁻ daga cikin maganin da sauri kuma ya riƙe shi da ƙarfi don a iya tantance carbon, a cire shi sannan a sake amfani da shi. Lambobi uku da ke jagorantar wannan aikin sune tauri (rayuwa a ƙarƙashin shear impeller), nau'in K/R (ƙarfi da gudu) da kuma raguwa (nawa carbon da aka ɗora ke niƙawa zuwa tarar da ba za a iya dawo da ita ba).

Maɓallin Takeaways

  • Tarar kuɗi tana ɗauke da zinare. Kowace gram na carbon da ke niƙawa a ƙasan allon yana barin da'irar da aka riga aka ɗora. Ragewa asarar murmurewa ce, ba kuɗin kula da gida ba.
  • Ana auna taurin ≥99%, ba a yi iƙirarin hakan ba. Taurin ƙwallon kwandon (ASTM D3802) da raguwar AARL suna ba da lambobi iri ɗaya a tsakanin masu samar da kayayyaki.
  • K yana saita ƙarfin aiki, R yana saita gudu. Carbon mai ƙimar K mai yawa amma ƙimar R mai rauni yana cika a hankali kuma yana barin zinariya ta wuce matakin sha na ƙarshe.
  • Ramin 6 × 12 shawara ce ta ruwa. Yanka mai tsauri yana hana rufe fuska tsakanin matakai yayin da yake kiyaye wurin da aka taɓa.
  • Toka ≤3.0% yana kare sake kunna zafi. Tokar ƙasa tana barin ƙananan ramuka masu tsabta bayan maimaita zagayowar murhu.
  • An gyara marufi. Jakunkunan PE masu nauyin kilogiram 25, danshi ≤5.0% kamar yadda aka cika, 15 MT MOQ ga kowace 1×20' FCL.
Bangaren da aka haɗa da takamaiman bayanai · Matsayin injiniyan AC50

Kayan Aiki: Kwakwa Shell granular Carbon da aka kunna · CAS 7440-44-0 · HS 3802.10 · Yawan yawa 0.48–0.55 g/ml · Marufi: 25 kg jakunkunan PE masu laminated masu nauyi · Sharuɗɗa: FOB ko CIF · MOQ 15 MT · Takardu: COA batch, TDS, MSDS.

sigaDarajar AC50Abin da yake sarrafawa
raga6 × 12Riƙe allo da wurin tuntuɓar juna
Taurin kwano≥99%Rayuwa a ƙarƙashin harsashin impeller
Ragewar Haihuwa (AARL)≤1.5%Asarar Carbon mai nauyi zuwa tara
Platelet≤5.0%Halin makantar allo
K darajar≥26 kg/tLoda zinare daidai gwargwado
Darajar R≥50%Adadin adsorption
CTC≥50%Alamar ƙarar micropore
Aikin butane≥19.5%Tabbatar da tsarin rami
Ash≤3.0%Tsaftacewar sake kunnawa
danshi≤5.0%Kwanciyar hankali bayan tafiye-tafiyen teku

Tsani mai daraja: BC1100 don cire tarin abubuwa da kuma aikin CIC (≥98.5% taurin) → AC50 don daidaitaccen CIP/CIL → AC55 (K ≥28 kg/t, R ≥55%) → AC60 (K ≥30 kg/t, R ≥60%, 8×16 ko 6×12). An cire lambar iodine da gangan daga wannan ƙayyadaddun bayanai har sai an tabbatar da adadi guda ɗaya; CTC da aikin Butane sune alamun ramuka da aka buga.

1. Abin da ke faruwa a cikin tankin shaye-shaye

Zinariya tana barin magudanar ruwa yayin da hadaddun auro cyanide Au(CN)₂⁻. Shafawa a kan harsashin kwakwa yana faruwa a matakai uku a jere: jigilar ta cikin fim ɗin ruwa da ke kewaye da granule, yaɗuwa cikin hanyar sadarwa ta rami, da kuma shawa ta zahiri a saman ciki. Mataki mafi jinkiri yana saita ƙimar da aka lura. A cikin tankin CIL mai cike da tashin hankali, fim ɗin ya zama siriri, don haka yaɗuwar rami da ɗaukar saman ya mamaye; a cikin ginshiƙin CIC mai ƙarancin tashin hankali fim ɗin na iya zama matsala.

Wannan shine dalilin da ya sa carbon guda biyu masu ƙarfin daidaitawa iri ɗaya suke yin aiki daban-daban a cikin ainihin shuka. Ƙimar K tana bayyana adadin zinare da tan ɗaya na carbon zai iya riƙewa a daidaito. Ƙimar R tana bayyana yadda yake kusantar wannan daidaiton da sauri. Da'irar da aka auna a kan K kawai za ta bi zinare a cikin mafita a matakin ƙarshe saboda carbon ɗin ba ya isa can a cikin lokacin zama da ake da shi.

Abincin kwakwa yana da mahimmanci a nan: yana samar da tsari mai ƙananan ramuka tare da ƙarfin injina mai yawa. Wannan haɗin yana ba da taurin da ake buƙata don tsira daga maimaita gwaje-gwaje, famfo da kuma zagayowar fitarwa yayin da yake riƙe da girman ramukan da ake buƙata don ɗaukar kaya cikin sauri.

2. Yanayin gazawa guda huɗu a cikin da'irar carbon

2.1 Ragewa da asarar zinare mai yawa

Masu tuƙi, famfo, masu wanke-wanke da kuma masu rufe duk wani abu mai kauri. Takardun da aka samu suna wucewa ta allon da ke ɗauke da zinare mai kauri kuma suna ɓacewa zuwa rafin wutsiya ko kuma zuwa ga ambaliya mai kauri. Saboda zinaren ya riga ya kasance a kan carbon, wannan asarar ba za a iya gani ba ga gwajin mafita na wutsiya - yana bayyana ne kawai a matsayin tazara tsakanin zinaren da aka narkar da shi da zinaren da aka dawo da shi.

2.2 Rufe allo daga abun cikin platelets

Platinum mai faɗi yana fuskantar ramukan allo kuma yana makantar da su da sauri fiye da granules masu daidaito. Screens masu makanta suna tilasta wucewa, da'ira ta gajeru da kuma rarraba carbon mara daidaito tsakanin matakai. Riƙe abun cikin platinum a ≤5.0% yana sa a iya hasashen zagayowar allo.

2.3 Tarin toka a tsakanin zagayowar sake kunnawa

Kowace sake kunna zafi tana barin ragowar da ba ta da sinadarai a cikin ramuka. Tokar farko mai yawa tana hanzarta raguwar yawan sha, don haka dole ne a maye gurbin carbon da wuri. Tokar ≤3.0% tana ƙara yawan amfani da zagayowar murhu kuma tana rage farashi mai inganci a kowace tan na ma'adinan da aka yi wa magani.

2.4 Guba daga sinadarai masu gina jiki da kuma sinadaran flotation

Masu ƙuraje, masu tarawa, mai da kayan ƙamshi suna shaƙewa sosai kuma suna mamaye ƙananan ramuka. Da'irar da ke canza sinadaran niƙa ko flotation na iya ganin raguwar ƙimar R ba tare da wani canji a cikin carbon da aka kawo ba. Gano sinadaran maganin kafin a ɗora alhakin gurɓataccen carbon.

3. Koyarwa: ma'aunin carbon na CIP/CIL mai matakai bakwai

  1. Saita yawan sinadarin carbon a kowane matakin shaƙa (g/L na ɓangaren litattafan almara) bisa ga girman tanki da nauyin zinare da aka yi niyya. Yi rikodin shi a matsayin kewayon, ba adadi ɗaya ba.
  2. Auna maganin tenor Shiga da fita daga kowane mataki. Bayanin mataki-mataki yana gaya maka inda shaƙar iska ke faruwa a zahiri.
  3. Lissafin nauyin ma'auni daga ƙimar K na matakin da aka zaɓa da kuma tenor na maganin da aka lura; kwatanta shi da gwajin carbon da aka auna.
  4. Duba motsi akan ƙimar R da ainihin lokacin zama a kowane mataki. Idan nauyin da aka auna ya ragu da ma'aunin daidaito, matakin yana da iyaka ga ƙimar aiki, ba iyaka ga iya aiki ba.
  5. Yi lissafin ƙimar gaba ta carbon Ana buƙatar kiyaye carbon da aka ɗora a ƙasa da iyakar ƙirar fitar da ruwa, daidaita kayan zinare da yawan fitar da ruwa.
  6. Kimanta asarar raguwa ta hanyar kwatanta kayan haɗin carbon da ƙirar ≤1.5%, sannan a mayar da ƙarancin zuwa zinare mai ɗauke da sinadarin carbon ta amfani da gwajin da aka ɗora.
  7. Rufe madauki tare da sake kunnawa. Da'irar log na murhu, yanayin toka da ƙimar R bayan kowace sabuntawa, sannan saita dokar maye gurbin daga raguwar da aka auna maimakon daga kalanda mai tsayayye.

Daidaiton aiki ya dogara ne akan tsire-tsire: yawan fitarwa, yawan ɓawon burodi, tenor na maganin da adadin matakai duk suna canza amsar. Hanyar ta kasance iri ɗaya; shigarwar ta fito ne daga kamfen ɗin ɗaukar samfur naka.

4. Teburin magance matsala

SymptomMai yuwuwa daliliDuba na farko
Zinare a matakin ƙarshe na mafitaShaƙatawa mai iyaka, ƙarancin ƙimar R ko kuma ɗan gajeren zamaBayanin mataki, lokacin zama, tashin hankali
Yawan amfani da sinadarin carbon mai yawaRage farashi sama da ƙira, famfo mai ƙarfiFines a wutsiya, saurin famfo, ƙirar canja wuri
Fuskokin allo suna makanta da wuriYawan platelet ko granules ɗin da suka lalaceRarraba siffar barbashi, buɗewar allo
Loda faɗuwa bayan canjin flotationGubar kwayoyin halitta ta microporesTsarin reagent, mafita TOC, sake gwajin ƙimar R
Ƙarfin aiki yana raguwa bayan zagayowar kilnTarin toka a cikin poresYanayin toka, yanayin zafin sake kunnawa
Rashin daidaiton carbon tsakanin matakaiKewaya allo ko rashin daidaiton ɗaga iskaBinciken kaya na mataki, ƙimar gaba

5. Zaɓin maki da takardar faffadan bayanai

wajibiGradeDabarun zaɓi
Tarin tsiri / ginshiƙin CICBC1100Ƙananan yankewa, dogon hulɗa, ≥98.5% tauri
Tsarin CIP / CIL na yau da kullunAC50Matsayin injiniya, K ≥26 kg/t, R ≥50%
Mafi girman ƙarfin aiki na CILAC55K ≥28 kg/t, R ≥55%
Babban aikin yankewa / babban aikin tenorAC60K ≥30 kg/t, R ≥60%, 8×16 ko 6×12

Shafawa yana faruwa ne bayan an narkar da shi a cikin takardar kwararar ruwa. AuCyan™ Sodium Cyanide NaCN (≥98.3%) ya rufe matakin zubar da ruwa ; inda aka fi son hanyar sinadarai ta gama gari, za a iya tabbatar da da'irar ta amfani da AuLeach™ Gold Leaching Agent (GDA) - Ba Mai Haɗari ba . Samun dukkan ukun daga masana'anta ɗaya yana sa yanayin gwaji, takardu da tsarin jigilar kaya su yi daidai.

Yanayin masana'antu · bayanan da suka gabata

Shirin AngloGold Ashanti na ranar 5 ga Nuwamba, 2026 na Brownfield ya ware dala miliyan 480–580 ga Geita da ke Tanzania, wanda ke nufin kimanin oz 600,000/y nan da shekarar 2030 idan aka kwatanta da oz 492,000 a shekarar 2025. Yawan fitar da iskar gas a kwata na uku na shekarar 2026 ya kai oz 120,000, raguwar kashi 4% a kowace shekara yayin da ma'aunin hakar ma'adinai ya ragu. Fadada tasirin iskar carbon da ke akwai yana kara zagayawa da aikin tantancewa maimakon gabatar da sabon tsarin masana'antu - wanda shine ainihin inda raguwar iskar gas, yanke raga da riƙe allo suka zama masu canji masu iko. Tushe: Sabuntawar kamfanin Q3 2026 da sanarwar faɗaɗawa, 5 ga Nuwamba, 2026.

6. Tambayoyi akai-akai

T1. Menene ainihin ma'aunin taurin ≥99%?
Taurin kwano, wanda aka gwada bisa ga ASTM D3802, yana auna juriya ga lalacewar injiniya a ƙarƙashin gogewar da aka sarrafa. Yana annabta yadda ƙwayoyin granules ke tsira daga impellers, famfo da kuma tantancewa.

T2. Me yasa raguwar kashi ≤1.5% matsala ce ta murmurewa maimakon matsalar kuɗi?
Domin tarar da ta karyewa ta riga ta cika da zinare. Suna wucewa ta allon kuma suna barin da'irar, don haka asarar ta bayyana a matsayin gibin dawowa maimakon kuɗin reagent.

T3. Menene bambanci tsakanin ƙimar K da ƙimar R?
K shine ƙarfin ɗaukar nauyin ma'auni a cikin kilogiram na zinariya a kowace tan na carbon; R shine ƙimar da carbon ke kusantar wannan daidaiton. Ƙarfin da ba shi da ƙimar yana barin zinariya a cikin ruwan magani.

T4. Me yasa za a ƙayyade yanke raga mai girman 6 × 12?
Rarrabawar ƙananan ƙwayoyin cuta tana hana allon daga makanta tsakanin matakai kuma tana ba da damar yin amfani da iskar hydraulic yayin da take kiyaye isasshen yanki na saman don sha.

T5. Ta yaya abun cikin platelet ke shafar da'irar?
Riƙe platelets ɗin da ke da faɗi yana ɗaure ramukan allo. Riƙe platelets a ≤5.0% yana sa zagayowar tantancewa ta kasance daidai kuma yana hana wucewa tsakanin matakan sha.

T6. Me yasa kuke buga ayyukan CTC da Butane maimakon lambar iodine?
Waɗannan su ne alamun ramuka da aka tabbatar don wannan matakin. Har sai an daidaita adadi ɗaya na aidin a duk takardun wurin, ƙayyadaddun ya dogara ne akan CTC ≥50% da Butane ≥19.5%.

T7. Menene toka ≤3.0% ke karewa?
Sake kunna zafi. Rage ragowar da ba na halitta ba yana barin ƙananan ramuka masu tsabta bayan kowace zagayowar murhu kuma yana rage raguwar yawan sha.

T8. Wane mataki ya kamata masana'antar CIL ta yau da kullun ta fara da shi?
AC50 shine matakin injiniyanci don aikin CIP/CIL na yau da kullun. Matsar zuwa AC55 ko AC60 lokacin da fitarwa, tenor ko shear ke buƙatar haɗin K/R mafi girma.

T9. Ta yaya ake tattara iskar carbon da jigilar ta?
A cikin jakunkunan PE masu nauyin kilogiram 25, danshi ≤5.0% kamar yadda aka cika, a 15 MT MOQ ga kowace 1 × 20' FCL a ƙarƙashin sharuɗɗan FOB ko CIF.

T10. Za a iya samar da samfuran gwajin dakin gwaje-gwaje?
Eh — Ana samun samfuran gwajin AuCarb™ da AuLeach™ don tabbatar da dakin gwaje-gwaje da kanka kafin a yi odar FCL.

T11. Me yasa kaya ke raguwa bayan wani abu mai kama da flotation reagent ya canza?
Masu tattarawa, masu tattarawa da mai suna mamaye ƙananan ramuka kuma suna rage yawan shaye-shayen da ke cikin su. Duba sinadaran maganin kafin a danganta digowar da wurin da ake amfani da sinadarin carbon.

T12. Waɗanne samfura ne suka cika sauran takardar bayanai?
AuCyan™ Sodium Cyanide NaCN (≥98.3%) don narkewa da kuma AuLeach™ Gold Leaching Agent (GDA) – Ba shi da haɗari ga hanyar fitar da sinadarai.

7. Karatun fasaha da hanyoyin haɗin ciki

Jagorar AuCarb™ · AC50 · AC55 · AC60 · BC1100 · Shafin farko na AC50 · Zinare Triangle · AuCyan™ · AuLeach™ GDA · Abubuwan da ke fitar da sinadarai · Tambayoyin da ake yawan yi game da sinadarai · Labaran Masana'antu

Nemi samfuran dakin gwaje-gwaje da kuma kimantawa

Tuntube Mu · WhatsApp +86 173 9270 5576 · info@unitedchemicalcn.com

  • Bazuwar Abun ciki
  • Abun ciki mai zafi
  • Abin dubawa mai zafi

Za ka iya kuma son

Tuntuɓar saƙon kan layi

Ƙara sharhi:

+ 8617392705576WhatsApp QR CodeDuba lambar QR
Bar sako don tuntuba
Na gode da sakon ku, za mu tuntube ku nan ba da jimawa ba!
Aika
Sabis na Abokin Ciniki ta Kan layi