Kedu mgbe Ụzọ Na-abụghị Cyanide Na-akwụ Ụgwọ n'ezie?

A bottle-roll decision method for AuLeach™ GDA covering pH, split dosing and the recovery-versus-cost trade-off.

White gold leaching agent powder on laboratory paper beside a sampling spoon

UNITED CHEMICAL · TEKNỌLỊKA NGWA AHỊA · 27 NỌVEMBER 2026

Onye na-abụghịcyanide route is a commercial decision, not a label

Peak recovery is the least important number in the decision.

Operations compare a leaching agent on peak recovery and stop there. The operating cost is actually set by pH, dosage and solution chemistry moving together. Ihe Nleta Ọlaedo AuLeach™ (GDA) - Ọ dịghị akpata nsogbu ụgbọ mmiri dị ka kemịkalụ a na-ahụkarị ma ejiri ya mee ihe na Obo leaching na Ịchụpụ VAT circuits where permissible cyanide use is constrained or supply chains are long. This guide sets out when the route pays and how to find out with a week of test work.

1. Three situations that favour the route

First, jurisdictions where cyanide permitting is constrained. Second, sites far from licensed cyanide supply chains. Third, ores where cyanide demand is uneconomic because of copper-bearing minerals. In each case the decision must be made on test work, not assumption.

Where cyanide remains the preferred route, AuCyan™ Sodium Cyanide NaCN (≥98.3%) is the reference reagent. The two routes are complementary; a technical team should be able to model both from the same ore sample.

2. Bottle-roll design

Use 1 kg of pulverised ore at 40% solids, three dosage levels plus a control, sampled at 2, 6, 12 and 24 hours. Record gold extraction, reagent consumption and pH drift at every point. The curve shape tells you whether the circuit is reagent-limited or kinetics-limited. If extraction plateaus early, more reagent buys nothing. If it is still climbing at 24 hours, contact time is the constraint.

agbanwensoNa-ekpughe
Nta35-45%Contact efficiency
Ọnụọgụ ọgwụAla / etiti / eluỌnụọgụ ego
pHOtu egwu kpọmkwem maka saịtị ahụWindo kwụsiri ike
TimeAwa 2 / 6 / 12 / 24Usoro Kinetics

3. Worked comparison: recovery versus cost per ounce

Suppose bottle rolls show 82% extraction with conventional cyanidation at 0.30 kg/t demand, and 74% with the non-cyanide route at 0.45 kg/t. On a 2,000 t/day ore at 1.5 g/t, the conventional route recovers 2,460 g/day of gold and the alternative 2,220 g/day — a 240 g/day difference. At US$3,550/oz that is roughly US$27,000/day of revenue. The reagent saving would have to exceed that to justify the switch. In a jurisdiction where cyanide permitting is constrained, the comparison changes because the alternative route is the only route available.

Ot: 82% at 0.30 kg/t

Non-cyanide: 74% at 0.45 kg/t

Recovery gap: ≈ 240 g/day ≈ US$27,000/day

4. pH is the master variable

pH governs reagent stability, gold surface chemistry and the behaviour of interfering species. Establish a site-specific setpoint from bottle-roll work and hold it with automatic control. In a Ịchụpụ VAT circuit, log pH at top, middle and bottom of each vat to detect stratification. Drift outside the agreed band shows up first as slower extraction, then as higher consumption.

5. Usoro nhazi nkewa na ikpere nke usoro ahụ

If the first half of the dose delivers 80% of extraction and the second half delivers 4%, the second half is buying inventory, not recovery. Split dosing with measurement lets you stop at the knee. On 2,000 t/day, trimming an unproductive 0.15 kg/t saves about 300 kg/day, roughly 110 t/year, with no change in gold output. The same discipline applies to free cyanide in a conventional circuit.

6. Heap and vat commissioning

n'ihi na Obo leaching, run column tests on each ore domain, control irrigation-solution pH and split the dose across irrigation stages. For Ịchụpụ VAT, run bottle rolls, control vat solution pH and split the dose across leach cycles. In both cases dissolved gold is recovered on AuCarb™ Gold Recovery Shell AuCarb™ Activated Carbon (≥99% Ike) selected on K and R values from the same test programme, typically in Kabọn-n'ime kọlụm service for clarified heap solutions.

7. Ntinye na akwụkwọ

AuLeach™ GDA ships as a common chemical with batch COA, TDS na MSDS, na Akpa PE dị arọ nke e ji ihe mkpuchi PE mee nke dị kilogram 25MOQ bụ 1 × 20' FCL ≈ 28 MT n'okpuru FOB / CIF usoro. United Chemical Na-eje ozi ihe karịrị mba 77. Ihe nlele AuLeach™ na AuCarb™ dị maka nnwale ụlọ nyocha onwe ha tupu e nye ha ngwaahịa.

8. Ajụjụ

Q1 — Nke a ọ bụ usoro na-abụghị nke cyanide?

Ee. AuLeach™ GDA bụ ihe na-anaghị eji amịpụta ọlaedo nke a na-enye dị ka kemịkalụ a na-ahụkarị.

Q2 — Do I need to rebuild the circuit?

Typically no; it is designed for existing Heap leaching and Vat leaching circuits, subject to test work.

Q3 — How is it described for handling?

As Non-Hazardous, with a batch COA, TDS and MSDS.

Q4 - Kedu ka m ga-esi họrọ dose ahụ?

From a three-level bottle-roll programme, stopping at the knee of the curve.

Q5 - Kedu MOQ na usoro?

1 × 20' FCL ≈ 28 MT, FOB ma ọ bụ CIF.

Q6 — Can gold be recovered on carbon?

Yes — AuCarb™ carbon in Carbon-in-Column or Carbon-in-Pulp service.

Run the route comparison

Send ore grade, pH data and circuit configuration. We return a bottle-roll protocol, a dosing curve and a landed-cost estimate.

Kpọtụrụ Anyị · Ihe ndị na-eme ka mmiri ghara ịpụ apụ · Nchịkọta ngwaahịa atọ · Ajụjụ Ndị A Na-ajụkarị gbasara kemịkalụ · Akụkọ Ụlọ Ọrụ

WhatsApp +86 173 9270 5576 · info@unitedchemicalcn.com

  • Ọdịnaya enweghị usoro
  • Ọdịnaya na-ekpo ọkụ
  • Ọdịnaya nyochaa na-ekpo ọkụ

Ị nwere ike na-amasị

Ndụmọdụ ozi ịntanetị

Tinye okwu:

+ 8617392705576Koodu QR WhatsAppNyochaa koodu QR
Hapụ ozi maka ntụle
Daalụ maka ozi gị, anyị ga-akpọtụrụ gị n'oge adịghị anya!
Nyefere