UNITED CHEMICAL · 行业新闻 · 2026年11月27日
A domestic process reaches a construction site
Sorption tank leaching puts sorbent quality at the centre of the design.
A subsoil user is building a gold recovery plant at the Ushtagan deposit in Kazakhstan using technology developed by VNIItsvetmet, the Ministry of Industry and Construction reported on 26 November, according to VRK News. The plant is designed to produce 0.8–0.9 tonnes of doré alloy a year. Institute scientists studied the Ushtagan ores and substantiated sorption tank leaching — gold dissolved in tanks and captured by a sorbent — then prepared the process specification on which the plant was designed.
1. Why sorption tank leaching is a reagent story
In tank sorption, the 碳 sits in the leach circuit and adsorbs gold as it dissolves. That places the sorbent in a mechanically aggressive environment while demanding both loading rate and capacity. 炭浆法(CIP) 和 炭浸法(CIL) practice is directly relevant: hardness and attrition determine fines generation, and K and R values determine how quickly and how heavily the carbon loads.
2. A process with a track record
The ministry noted that VNIItsvetmet technology was used at Sekisovskoye in 2008 with sorption leaching, at Severny Raigorodok in 2009 with heap leaching of weathering-crust ores, and at Sharyk in 2014. That history matters to a supplier: an ore-matched process specification usually means the plant has already defined its reagent and sorbent requirements before construction. Qualification work therefore centres on matching a commercial product to the specified method, not on redesigning the flowsheet.
金三角——三种产品,一家供应商
AuCyan™ 氰化钠 (NaCN) (≥98.3%) · AuCarb™ 黄金回收椰壳活性炭 (≥99% 硬度) · AuLeach™ 黄金浸出剂 (GDA) – 无害
3. Worked sizing check
At 0.8–0.9 tonnes of doré a year, roughly 26,000–29,000 ounces of gold are recovered annually. If the circuit runs at 85% recovery, the contained gold in feed is around 31,000–34,000 ounces. A carbon inventory sized on tank volume rather than annual ounces is the correct approach; the annual figure is useful for estimating make-up. At 0.05 kg/t make-up and 1,000 t/day, annual carbon demand is about 18 tonnes — just over one 15 MT container.
Doré target: 0.8–0.9 t/year ≈ 26,000–29,000 oz
碳组成成分示意图: ≈ 18 吨/年
4. Product fit for a tank-sorption plant
AuCyan™ 氰化钠 NaCN (≥98.3%) supplies the leaching step at 18 MT per container under licensed import. AuCarb™ 黄金回收椰壳活性炭(硬度≥99%) is the sorbent candidate, specified at ball-pan ≥99% and AARL attrition ≤1.5% at 15 MT 每个容器。 AuLeach™黄金浸出剂(GDA)——无害 is evaluated where permitted at 28 MT. All ship with batch COA, TDS 和 MSDS认证在 25公斤重型复合聚乙烯袋,下 离岸价/到岸价 条款。
3b. Doré is not finished gold
The reported 0.8–0.9 tonnes a year is doré alloy, an intermediate bar of gold and silver that must be refined before it becomes pure metal. That distinction matters for reagent planning because doré weight includes silver, so the contained gold is lower than the headline tonnage suggests. It also matters for the carbon circuit: a polymetallic feed changes loading behaviour and can raise reagent demand through silver and base-metal competition. A qualification programme should therefore use a representative composite of the actual Ushtagan ore, not a generic low-grade standard. The same principle applies to the sorbent: 纸浆炭 和 浸出碳 grades are selected on K and R values measured with site solution, and those values move when the solution chemistry changes.
3c. Why doré tonnage needs a second look
The reported 0.8 to 0.9 tonnes a year is doré alloy, an intermediate bar of gold and silver that must be refined before it becomes pure metal. The headline tonnage includes silver, so contained gold is lower than a simple reading suggests. That matters for reagent planning in two ways. A polymetallic feed changes carbon loading behaviour and can raise reagent demand through silver and base-metal competition. And a qualification programme should use a representative composite of the actual Ushtagan ore rather than a generic low-grade standard. 纸浆炭 和 浸出碳 grades are selected on K and R values measured with site solution, and those values move when solution chemistry changes. A dossier built on the real ore is the only one that survives commissioning.
5。 常问问题
Q1 — What is being built?
A gold recovery plant at Ushtagan using sorption tank leaching technology.
Q2 — What is the design output?
0.8–0.9 tonnes of doré alloy a year.
Q3 — Who developed the process?
VNIItsvetmet, a Kazakh research institute.
Q4 — Which carbon grade fits tank sorption?
One with documented hardness, attrition, K and R values matched to the ore.
Q5 — What terms apply?
FOB or CIF with batch COA, TDS and MSDS.
Q6 — Do you serve Central Asia?
Yes — more than 77 countries, including Central Asian markets.
Match a sorbent to your process spec
Send your process specification and ore data. We return a carbon and reagent dossier for tank sorption.
WhatsApp +86 173 9270 5576 info@unitedchemicalcn.com
Source: VRK News, 26 November 2026, citing Kazakhstan's Ministry of Industry and Construction.