The Carbon you replace is not the carbon you lose

Fines carry gold out of the circuit, and they rarely appear on the purchase order.

Activated carbon is consumed two ways. It leaves as loaded carbon after elution, and it grinds into fines that report to tailings carrying adsorbed gold. The second loss is rarely budgeted. Ball-pan hardness and AARL attrition predict it; mesh size and platelet count predict how fast it happens in a given circuit. This guide uses AuCarb™ Gold Recovery Coconut Shell Activated Carbon (≥99% Hardness) as the worked example.

1. Three steps from solution to loaded carbon

Film diffusion — the [Au(CN)₂]⁻ complex crosses the solution boundary layer around each granule. Agitation controls this step.

Pore diffusion — the complex travels into internal pores. Granule size and pore structure control this step.

Surface adsorption — the complex binds to active sites. Surface chemistry and total area control this step.

2. Why hardness is a recovery parameter

A granule that breaks in a stirred tank shortens diffusion paths but creates gold-bearing fines that escape the adsorption circuit. In an abrasive ore, moving from a marginal product to one at ball-pan hardness ≥99% with AARL attrition ≤1.5% cuts fines generation directly. The AC50 verified data set is: 6×12 mesh, ball-pan ≥99%, AARL attrition ≤1.5%, platelet ≤5.0%, K ≥26 kg/t, R ≥50%, CTC ≥50%, butane ≥19.5%, ash ≤3.0%, moisture ≤5.0%, bulk density 0.48–0.55 g/mL. Iodine value is deliberately omitted — published figures conflict, so CTC and butane activity are the auditable measures.

3. Worked calculation: the cost of fines

A 2,000 t/day CIL plant carries 12 tonnes of carbon with a 30-day cycle. At 1.5% attrition per cycle it loses about 180 kg per cycle, or 2.2 tonnes a year. At 3.0% it loses roughly 4.3 tonnes — a difference of 2.1 tonnes of carbon. If those fines carry even 200 g/t of gold, the annual gold difference is about 420 g. At any reasonable gold price, the hardness premium paid for the better carbon is smaller than the gold saved.

1.5% attrition: ≈ 2.2 t/year make-up carbon

3.0% attrition: ≈ 4.3 t/year make-up carbon

4. K and R are not the same number

K value is the adsorption rate constant — how fast gold loads. R value is equilibrium capacity — how much it holds. A high K with modest R suits short contact time. A high R suits a circuit that runs carbon to heavy loading before elution. Buying on either alone is a common and expensive mistake. Run bottle-roll loading on your own ore, set the K/R target from your contact time, then buy the lowest grade that reaches it.

5. Four grades, four jobs

GradeCircuitDefining spec
BC1100Heap leaching / Carbon-in-ColumnHigh activity for lower-grade solutions
AC50Standard CIP/CIL6×12 mesh, K ≥26, R ≥50%, CTC ≥50%
AC55Higher-loading CIP/CILK ≥28 kg/t, R ≥55%
AC60Premium CIP/CILK ≥30 kg/t, R ≥60%, 8×16 or 6×12

6. Regeneration and cycle life

Loaded carbon is eluted and thermally regenerated before returning to the circuit. Every cycle imposes thermal and mechanical stress. Platelets and weak granules are preferentially lost in handling and regeneration. A carbon at ball-pan hardness ≥99% with platelet ≤5.0% typically sustains more cycles before make-up is required. Packing is 25 kg heavy-duty laminated PE bags, with a batch COA, TDS and MSDS. MOQ is 1×20' FCL ≈ 15 MT under FOB/CIF terms; United Chemical serves more than 77 countries.

5b. Screening and fines recovery

Attrition control does not end at the carbon specification. Screen condition determines whether a broken granule is removed cleanly or ground further and carried forward. A worn screen with oversized apertures passes loaded fines into the tailings stream; a blinded screen holds carbon in the tank too long and increases grinding. The practical routine is to log screen aperture, inspect panels on a fixed schedule and sample the carbon size distribution in the circuit monthly. If the proportion of sub-millimetre material is rising while make-up carbon is on budget, the problem is mechanical rather than metallurgical. Equally, gold-bearing fines caught on a screen are not lost; they should be routed to the elution circuit where the recovery economics justify it. This is why hardness and attrition numbers belong in an operating dashboard, not only in the purchase order.

7. FAQ

Q1 — What does ≥99% hardness mean in practice?

Ball-pan hardness ≥99% means the granule resists mechanical breakdown to a defined standard, reducing fines.

Q2 — Which mesh size?

6×12 for agitated CIP/CIL, 8×16 where finer loading is needed, BC1100 for columns and heap.

Q3 — Do you publish iodine value?

No — CTC and butane activity are the auditable pore measures because published iodine figures conflict.

Q4 — What ships with each batch?

Batch COA, TDS and MSDS in 25 kg heavy-duty laminated PE bags.

Q5 — What is the MOQ?

1×20' FCL ≈ 15 MT, FOB or CIF.

Q6 — Can I test before buying?

Yes — complimentary samples of AuCarb™ and AuLeach™ for independent laboratory testing.

Measure your attrition loss

Tell us your circuit type, screen aperture and ore abrasiveness. We propose a grade, a K/R target and a test protocol.

Contact Us · AC50 · AC55 · AC60 · Golden Triangle overview

WhatsApp +86 173 9270 5576 · info@unitedchemicalcn.com

You may also like

Online message consultation

Add comment:

+8617392705576WhatsApp QR CodeScan QR code
Leave a message for consultation
Thanks for your message, we will contact you soon !
Submit